Aesthetic ceramic coating applied over a baked resistant substructure based on ultra hard zircon and sodium oxide.
Enamel imitates the incisive transparency of enamel.
It is applied on top of the dentine mass. When applying the Enamel for the first time, you should focus on the adjacent teeth and restore the necessary anatomy of the restoration by 10% more than the desired result.
Dentin, Enamel, Clear, Neutral, Translucent, Modifier, Chroma, Mamelon, Gingiva
Coefficient of thermal expansion |
2 firing: 9.0 x 10-6 x K-1; 4 firing: 9,0 x 10-6 x K-1 |
Conversion temperature |
500°C ±10 |
Stain Powder Dye
Coefficient of thermal expansion |
9,8 x 10-6 x K-1; |
Conversion temperature |
510°C ±10 |
Opal Opal
Coefficient of thermal expansion |
2 firing: 12.5 – 13.5 x 10-6 x K-1; 4 firing: 12,5 – 13,5 x 10-6 x K-1 |
Conversion temperature |
500°C ±10 |
| ZR (zirconium ceramics) | t° preheating | Drying time | t° of the beginning of the vacuum mode | Warm-up rate | Firing | Exposure time |
|---|---|---|---|---|---|---|
| Cleaning roasting | 500° C | 3 min. | 500° C | 65° C / min. | 980° C | 5 min. |
| 1st firing
Dentin / Enamel |
450° C | 6 min. | 450° C | 45° C / min. | 810° C | 1 min. |
| 2nd firing
Dentin / Enamel |
450° C | 6 min. | 450° C | 45° C / min. | 810° C | 1 min. |